Thermoplastic polyurethane
TPU
Flexible, rubber-like. The number (95A, 85A) is shore hardness, lower is softer. Print slowly, direct drive preferred.
- Nozzle
- 210–240 °C · 190–240 °C on shelves
- Bed
- 30–60 °C
- Dry
- 50 °C · 6 h
- Enclosure
- no
On plates
| Surface | Bed | Between |
|---|---|---|
| Textured PEI | 30–50 °C | none |
| Smooth PEI | 30–50 °C | release |
| Cool Plate | 30–35 °C | none |
| Engineering | 30–40 °C | glue stick |
| Glass | 40–60 °C | glue stick |